personal lux
Well-Known Member
So ive got myself quite a set up of extractors from best value vacs. Im currently running 2 closed column dewax units, one 1.5" 1/2lb , 1 3" 1lb. ive basically been running them ass a closed column open blast and Im looking to upgrade this system with a molecular sieve set up, and also to begin running my 1lb system with no material with extra steel barrings and filters only as a true dewaxing column after a 2lb material column. Im SUPER curious as of what i can do to remove ANY excess moisture from my material before or during the extraction due to living here in michigan our humidy can be quite annoying! Im considering running my 1.5"x12" column as my sieve column before the butane goes into the extractor, and also when it comes back into the recovery tank. Do i need to run the tank at room temp before the sieve, and then cool it with a coil before it goes into my material tube or is cold fine? Any suggestions and questions to help me explain more in depth are appreciated and ill answer as quickly as possible!