Alright gonna be postin quite a few photos.
teflon don tek haha
Side purge til i get the vac oven. Cant wait to just lay the sheet flat and get a smaller muffin.
Worked pretty well but we couldnt put it on heat so we could only get so far.
After the main muffin dropped i was able to toss it in the chamber the normal way without worrying about it getting out of control.
All folded up after about 12 hours purging. Really came off the teflon well this time. Gotta make sure to fold before 24+ hours depending on strain or itll be too stable to easily get it to stick to itself. Depending on strain of course.
Now inspecting for hairs/foreign material. Gotta get one of those beard nets for myself. Luckily most of what i make goes to me so while i keep it clean im much more relaxed about a tiny flake of trim in a corner or some slight buddering or a hair laying on the surface that i can pick off. I try for shatter but like all forms as long as clean and well purged.
And i cant seem to find any of the finished slab pictures. Gotta check my hd and shit. Always puttin shit into random folders.